I like to mount my figures on steel washers, as I've mentioned before. That often means I have to extend the figure's base so that it doesn't look like it's just been plonked down on the washer.

Normally I use Green Stuff, but that takes an age to cure, and I don't really have as much patience as I ought. So I've been looking around for something that I can model easily and that cures quickly. Super Sculpey seems to fit the bill nicely.

It doesn't cure without being exposed to heat (130°C, 15 minutes per 6mm thickness), so I can take my time with modelling, unlike with fast-cure epoxy putties. I was a bit unsure whether the heat would be too much for a plastic miniature, but it seems to be fine: the Bonesium does get soft and wobbly, but the low temperature required to cure the Sculpey doesn't come close to melting it.

The only issue I've found with using Sculpey, as opposed to Green Stuff, is that it doesn't stick to the plastic very well at all. That's not a huge problem though, and I can see times when it would be a positive advantage.

 

Note: I'm not sure how much use this photograph really is; sculpey and bonesium are both a huge pain to photograph in detail, both being ever-so-slightly translucent. Ah well, there it is for what it's worth.

Edited by MojoBob
  • Like 6
Link to comment
Share on other sites

  • Replies 4
  • Created
  • Last Reply

Top Posters In This Topic

Top Posters In This Topic

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Restore formatting

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...